G5(F3X)
High shrink ratio polyolefin tubing
Technical Data |
Property
|
Test
Method
|
Typical
Data
|
Tensile
Strength
|
ASTM
D 2671
|
14
MPa
|
Elongation
at break
|
ASTM
D 2671
|
800
%
|
Tensile
strength after aging at 175℃ for 168 hrs.
|
ASTM
D 2671
|
14
MPa
|
Elongation
after aging at 175℃ for 168 hrs.
|
ASTM
D 2671
|
350
%
|
Flammability
|
UL
224 VW-1
SAE-AMS-DTL-23053/5
|
Pass
|
Heat
shock (250℃/4hrs.)
|
ASTM
D 2671
|
No
cracking
|
Cold
bend test (-55℃/4hrs.)
|
ASTM
D 2671
|
No
cracking
|
Dielectric
strength
|
ASTM
D 150
|
20KV/mm
|
Volume
resistance
|
ASTM
D 876
|
1014Ω․cm
|
Copper
Corrosion
|
UL
224
|
Pass
|
Water
absorption
|
ASTM
D 570
|
0.15%
|
Chemical
resistance
|
SAE-AMS-DTL-23053/5
|
Pass
|
Longitudinal
shrinkage
|
UL
224
|
0±5%
|
Eccentricity
|
UL
224
|
30%
|
|
|